Kobs India is involved in offering a widespread range of Incoloy Forged Bushing Fittings at reasonable prices to our clienteles. As a supplier, manufacturer, stockiest, and exporter, we offer this Incoloy Forged Bushing Fittings in different sizes and thickness. It is a fitting used to joint two threaded items of different size. There are a lot of different applications in which forged steel pipe fittings would be ideal.
These round head bushing come in one piece body design and the trouble-free to put back congregation make these industrial pipe fittings extremely uncomplicated to clean and maintain. Our Forged Pipe Bushing is easy and cost-effective method to plug your pipe. Meanwhile, these fittings can further be customized in terms of sizes and thicknesses as per specific requirements given by our esteemed clients. We offer the same in market leading prices These include, but are not limited to; oil, gasoline, hydraulic machinery, fertilizing, or chemical industries. Because of the leak free connections created from fittings made from forged steel, these forged fittings are ideal in the transfer of these potentially harmful materials.
Meanwhile, our products are can further be made-to-order as per the detailed requirements given by our valuable clienteles.
Incoloy : Grade: Incoloy 800(2.4958), Incoloy 800H, Incoloy 800HT |
Incoloy | 800(2.4958) | 800H | 800HT |
Ni | 30-35 | 30-35 | 30-35 |
Fe | 39.5 min | 39.5 min | 39.5 min |
Cr | 19-23 | 19-23 | 19-23 |
Cu | 0.75 max | 0.75 max | 0.75 max |
Ti | 0.15-0.60 | 0.15-0.60 | 0.25-0.60 |
Al | 0.15-0.60 | 0.15-0.60 | 0.85-1.20 |
C | 0.1 max | 0.05-0.1 | 0.06-0.1 |
Mn | 1.5 max | 1.5 max | 1.5 max |
S | 0.015 max | 0.015 max | 0.015 max |
Si | 1.0 max | 1.0 max | 1.0 max |
Density | 7.94 g/cm3 |
Melting Point | 1385 °C (2525 °F) |
Tensile Strength | Psi – 75,000 , MPa – 520 |
Yield Strength (0.2%Offset) | Psi – 30,000 , MPa –205 |
Elongation | 30 % |
Stainless Steel : Grade: 304 (1.4301), 304L(1.4307), 304H (1.4948), 309 (1.4828), 309S, 310, 310S (1.4845), 316( 1.4401), 316H, 316L ( 1.4404 /1.4432) , 317, 317L (1.4438), 321 (1.4541), 321 H(1.4878), 347 (1.4550), 347H (1.4961), 904L (1.4539) Duplex Steel: Grade: 2205 (1.4507) Super Duplex Steel: Grade: 2507 (UNS S32750) Inconel : Grade: Inconel 600 (2.4640), Inconel 601 (2.4851), Inconel 625 (2.4856), Inconel 718(2.4668) Nickel : Grade: Nickel 200, Nickel 201 Titanium : Grade: Gr.1 (3.7025) , Gr.2 (3.7035) , Gr.3(3.7055) , Gr.5(3.7164/65), Gr. 7(3.7235) , Gr. 11 (3.7225) Monel : Grade: Monel 400, Monel K500 (2.4375), Monel R-405 Hastalloy : Grade: Hastalloy B2, Hastalloy B3, Hastalloy C22, Hastalloy C276, Hastalloy X |
The principal methods of hot working are extrusion, drawing, forging and rolling. Rolling is the most extensive employed forming process, though some limitations may apply to the process. Rolling mainly consists of three major sub-categories: flat rolling, shape rolling (with specifically designed roll grooves) and pipe rolling (including piercing). Forging may be sub-categorized as hamming, pressing, etc. .
Forging may be performed under hammers, in mechanical presses and upsetters or by a method known as roll forging. Pressing generally includes the manufacture of forged articles in hydraulic presses. Extrusion usually is performed in hydraulic presses which force the hot steel through a die. Rolling is performed in rolling mills of a variety of types. .
The two principal reasons for perform metal forming at elevated temperatures (hot working) are to reduce the forming loads through the reduction of the resistance of the steel to deformation, and to develop preferred metallurgical structures for strength and ductility of the finish products.
The most appropriate manufacturing method of a product will be decided with consideration of its material, sizes, shape, use, standards and other properties.